Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (33) Inactive Alloys (6) U.S. EPA Registered Antimicrobial (5) You Searched For: coated-metal-arc-welding:"Not Recommended" melting-point-solidus:[1600 TO 1650] CLEAR this search X SAVE this search << Page 1 >> 39 Alloys Found Alloy UNS#DesignationActiveView C27451 Yellow Brass (Yellow Brass) Yes C27451 Profile Suppliers of C27451 C27453 Copper Zinc Alloy Yes C27453 Profile Suppliers of C27453 C27460 Yes C27460 Profile Suppliers of C27460 C28000 * Muntz Metal, 60% Yes C28000 Profile Suppliers of C28000 C28340 Yes C28340 Profile Suppliers of C28340 C28500 Copper-Zinc- Alloy (Brass) Yes C28500 Profile Suppliers of C28500 C33200 High Leaded Brass (Tube) Yes C33200 Profile Suppliers of C33200 C33500 Low-Leaded Brass Yes C33500 Profile Suppliers of C33500 C34000 Medium Leaded Brass, 64-1/2% Yes C34000 Profile Suppliers of C34000 C34200 High Leaded Brass, 64-1/2% Yes C34200 Profile Suppliers of C34200 C34500 Yes C34500 Profile Suppliers of C34500 C35000 Medium Leaded Brass, 62% Yes C35000 Profile Suppliers of C35000 C35300 High Leaded Brass, 62% Yes C35300 Profile Suppliers of C35300 C35600 Extra High Leaded Brass Yes C35600 Profile Suppliers of C35600 C36000 Free-Cutting Brass Yes C36000 Profile Suppliers of C36000 C36010 Leaded Brass (Free-Cutting Brass) Yes C36010 Profile Suppliers of C36010 C36200 Leaded Brass No C36200 Profile Suppliers of C36200 C36300 Copper-Zinc-Lead Alloy Yes C36300 Profile Suppliers of C36300 C36500 Leaded Muntz Metal, Uninhibited Yes C36500 Profile Suppliers of C36500 C36600 Leaded Muntz Metal, Arsinical No C36600 Profile Suppliers of C36600 C36700 Leaded Muntz Metal, Antimonial No C36700 Profile Suppliers of C36700 C36800 Leaded Brass No C36800 Profile Suppliers of C36800 C37000 Free-Cutting Muntz Metal Yes C37000 Profile Suppliers of C37000 C37100 Yes C37100 Profile Suppliers of C37100 C37700 Forging Brass Yes C37700 Profile Suppliers of C37700 C38500 Architectural Bronze Yes C38500 Profile Suppliers of C38500 C44300 * Admiralty, Arsenical Yes C44300 Profile Suppliers of C44300 C44400 * Admiralty, Antimonial Yes C44400 Profile Suppliers of C44400 C44500 * Admiralty, Phosphorized Yes C44500 Profile Suppliers of C44500 C46400 Naval Brass, Uninhibited Yes C46400 Profile Suppliers of C46400 C46500 Naval Brass, Arsenical Yes C46500 Profile Suppliers of C46500 C46600 Tin Brass No C46600 Profile Suppliers of C46600 C46700 Tin Brass No C46700 Profile Suppliers of C46700 C48200 Naval Brass, Medium Leaded Yes C48200 Profile Suppliers of C48200 C48500 Naval Brass, High Leaded Yes C48500 Profile Suppliers of C48500 C68300 * Copper-Znc Alloy (Silicon Modified Brass) Yes C68300 Profile Suppliers of C68300 C85500 Yes C85500 Profile Suppliers of C85500 C85800 Yes C85800 Profile Suppliers of C85800 C87900 Copper Silicon Yes C87900 Profile Suppliers of C87900 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>