Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (31) Inactive Alloys (3) U.S. EPA Registered Antimicrobial (14) You Searched For: capacity-for-being-hot-formed:"Excellent" brazing:"Good" element_names:"Zinc" CLEAR this search X SAVE this search << Page 1 >> 34 Alloys Found Alloy UNS#DesignationActiveView C12510 * Yes C12510 Profile Suppliers of C12510 C19002 * Yes C19002 Profile Suppliers of C19002 C28550 Yes C28550 Profile Suppliers of C28550 C36500 Leaded Muntz Metal, Uninhibited Yes C36500 Profile Suppliers of C36500 C36600 Leaded Muntz Metal, Arsinical No C36600 Profile Suppliers of C36600 C36700 Leaded Muntz Metal, Antimonial No C36700 Profile Suppliers of C36700 C36800 Leaded Brass No C36800 Profile Suppliers of C36800 C37000 Free-Cutting Muntz Metal Yes C37000 Profile Suppliers of C37000 C37100 Yes C37100 Profile Suppliers of C37100 C37700 Forging Brass Yes C37700 Profile Suppliers of C37700 C38500 Architectural Bronze Yes C38500 Profile Suppliers of C38500 C46270 Yes C46270 Profile Suppliers of C46270 C46750 Yes C46750 Profile Suppliers of C46750 C49300 * Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile Suppliers of C49300 C49350 * Bismuth Brass Alloy Yes C49350 Profile Suppliers of C49350 C50590 * Yes C50590 Profile Suppliers of C50590 C50705 * Yes C50705 Profile Suppliers of C50705 C64760 * Yes C64760 Profile Suppliers of C64760 C65400 Yes C65400 Profile Suppliers of C65400 C67400 Yes C67400 Profile Suppliers of C67400 C67420 Yes C67420 Profile Suppliers of C67420 C68300 * Copper-Znc Alloy (Silicon Modified Brass) Yes C68300 Profile Suppliers of C68300 C68370 Yes C68370 Profile Suppliers of C68370 C69230 * Yes C69230 Profile Suppliers of C69230 C69240 Yes C69240 Profile Suppliers of C69240 C69300 * ECO Brass Yes C69300 Profile Suppliers of C69300 C69310 * SnEco Yes C69310 Profile Suppliers of C69310 C69350 Yes C69350 Profile Suppliers of C69350 C69850 Yes C69850 Profile Suppliers of C69850 C70310 * Yes C70310 Profile Suppliers of C70310 C70315 STOL 94 Yes C70315 Profile Suppliers of C70315 C87860 * Yes C87860 Profile Suppliers of C87860 C87870 * Yes C87870 Profile Suppliers of C87870 C87950 Yes C87950 Profile Suppliers of C87950 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>