Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (20) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (20) You Searched For: elongation:[39 TO 42] oxyacetylene-welding:"Fair" CLEAR this search X SAVE this search << Page 1 >> 20 Alloys Found Alloy UNS#DesignationActiveView C10100 * Oxygen-Free-Electronic (OFE) Yes C10100 Profile Suppliers of C10100 C10200 * Oxygen-Free (OF) Yes C10200 Profile Suppliers of C10200 C10300 * Oxygen-Free Copper (OFXLP) Yes C10300 Profile Suppliers of C10300 C10400 * Oxygen-Free with Ag (OFS) Yes C10400 Profile Suppliers of C10400 C10500 * Oxygen-Free with Ag (OFS) Yes C10500 Profile Suppliers of C10500 C10700 * Oxygen-Free with Ag (OFS) Yes C10700 Profile Suppliers of C10700 C10910 * Yes C10910 Profile Suppliers of C10910 C12000 * Phosphorus-Deoxidized, Low Residual P (DLP) Yes C12000 Profile Suppliers of C12000 C12100 * Phosphorus-Deoxidized, Low Residual P (DLPS) Yes C12100 Profile Suppliers of C12100 C14500 * Tellurium-Bearing (PTE) Yes C14500 Profile Suppliers of C14500 C14510 * Tellurium-Bearing Yes C14510 Profile Suppliers of C14510 C14520 * Phosphorus-Deoxidized,Tellurium-Bearing (DPTE) Yes C14520 Profile Suppliers of C14520 C41100 * Tin Brass Yes C41100 Profile Suppliers of C41100 C41120 * Yes C41120 Profile Suppliers of C41120 C50725 * Yes C50725 Profile Suppliers of C50725 C50780 * Yes C50780 Profile Suppliers of C50780 C52100 * Phospher Bronze, 8% C Yes C52100 Profile Suppliers of C52100 C70400 * Copper-Nickel, 5% Yes C70400 Profile Suppliers of C70400 C70600 * Copper-Nickel, 10% Yes C70600 Profile Suppliers of C70600 C71000 * Copper-Nickel, 20% Yes C71000 Profile Suppliers of C71000 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>