Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (38) Inactive Alloys (3) U.S. EPA Registered Antimicrobial (29) You Searched For: tensile-strength:[130 TO 140] CLEAR this search X SAVE this search << Page 1 >> 41 Alloys Found Alloy UNS#DesignationActiveView C17460 * Copper Beryllium Yes C17460 Profile Suppliers of C17460 C17465 Copper Beryllium Yes C17465 Profile Suppliers of C17465 C17540 CW103C Yes C17540 Profile Suppliers of C17540 C19050 * SPKFC-5E (High Copper) Yes C19050 Profile Suppliers of C19050 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C44250 * Yes C44250 Profile Suppliers of C44250 C44750 * Tin Brass Yes C44750 Profile Suppliers of C44750 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C52100 * Phospher Bronze, 8% C Yes C52100 Profile Suppliers of C52100 C52180 * Yes C52180 Profile Suppliers of C52180 C52480 * Yes C52480 Profile Suppliers of C52480 C53800 Yes C53800 Profile Suppliers of C53800 C61500 * Yes C61500 Profile Suppliers of C61500 C61800 * Yes C61800 Profile Suppliers of C61800 C61900 * Yes C61900 Profile Suppliers of C61900 C63800 * Yes C63800 Profile Suppliers of C63800 C64400 * Aluminum Bronze No C64400 Profile Suppliers of C64400 C64727 * Copper Silicon Alloy (MAX375) Yes C64727 Profile Suppliers of C64727 C64728 * Copper-Nickel-Zinc-Silicon Alloy Yes C64728 Profile Suppliers of C64728 C64751 Yes C64751 Profile Suppliers of C64751 C64752 Yes C64752 Profile Suppliers of C64752 C65400 Yes C65400 Profile Suppliers of C65400 C66930 * Copper-Manganese Alloy Yes C66930 Profile Suppliers of C66930 C69000 * Copper Zinc No C69000 Profile Suppliers of C69000 C69750 Yes C69750 Profile Suppliers of C69750 C70252 * Copper Nickel (NKC 388) Yes C70252 Profile Suppliers of C70252 C70255 Yes C70255 Profile Suppliers of C70255 C70330 Yes C70330 Profile Suppliers of C70330 C70345 Yes C70345 Profile Suppliers of C70345 C70350 * Yes C70350 Profile Suppliers of C70350 C70370 * Yes C70370 Profile Suppliers of C70370 C70390 Yes C70390 Profile Suppliers of C70390 C72660 * Yes C72660 Profile Suppliers of C72660 C72670 Yes C72670 Profile Suppliers of C72670 C72800 * Yes C72800 Profile Suppliers of C72800 C72900 * Yes C72900 Profile Suppliers of C72900 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 C96800 * Yes C96800 Profile Suppliers of C96800 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>