63 Alloys Found

Alloy UNS#DesignationActiveView

C10100 *

Oxygen-Free-Electronic (OFE) Yes C10100 Profile
Suppliers of C10100

C10200 *

Oxygen-Free (OF) Yes C10200 Profile
Suppliers of C10200

C10400 *

Oxygen-Free with Ag (OFS) Yes C10400 Profile
Suppliers of C10400

C10500 *

Oxygen-Free with Ag (OFS) Yes C10500 Profile
Suppliers of C10500

C10700 *

Oxygen-Free with Ag (OFS) Yes C10700 Profile
Suppliers of C10700

C11000 *

Electrolytic Tough Pitch (ETP) Yes C11000 Profile
Suppliers of C11000

C11100 *

Electronic Tough Pitch, Anneal Resistant (ETP) Yes C11100 Profile
Suppliers of C11100

C11300 *

Tough Pitch with Ag (STP) Yes C11300 Profile
Suppliers of C11300

C11400 *

Tough Pitch with Ag (STP) Yes C11400 Profile
Suppliers of C11400

C11500 *

Tough Pitch with Ag (STP) Yes C11500 Profile
Suppliers of C11500

C11600 *

Tough Pitch with Ag (STP) Yes C11600 Profile
Suppliers of C11600

C12500 *

Fire-Refined Tough Pitch (FRTP) Yes C12500 Profile
Suppliers of C12500

C12700 *

Copper Alloy No C12700 Profile
Suppliers of C12700

C12800 *

Copper Alloy No C12800 Profile
Suppliers of C12800

C12900 *

Fire-Refined Tough Pitch with Ag (FRSTP) Yes C12900 Profile
Suppliers of C12900

C13000

Copper Alloy No C13000 Profile
Suppliers of C13000

C15000 *

Zirconium Copper Yes C15000 Profile
Suppliers of C15000

C15100 *

Yes C15100 Profile
Suppliers of C15100

C15500 *

Yes C15500 Profile
Suppliers of C15500

C17200 *

Beryllium Copper Yes C17200 Profile
Suppliers of C17200

C18060

Yes C18060 Profile
Suppliers of C18060

C18100

Yes C18100 Profile
Suppliers of C18100

C18625 *

HRSC Yes C18625 Profile
Suppliers of C18625

C18835 *

Yes C18835 Profile
Suppliers of C18835

C19000 *

Yes C19000 Profile
Suppliers of C19000

C19200 *

Yes C19200 Profile
Suppliers of C19200

C19210 *

Yes C19210 Profile
Suppliers of C19210

C19215 *

Yes C19215 Profile
Suppliers of C19215

C19217

Yes C19217 Profile
Suppliers of C19217

C19220 *

Yes C19220 Profile
Suppliers of C19220

C19400 *

Yes C19400 Profile
Suppliers of C19400

C19720 *

Yes C19720 Profile
Suppliers of C19720

C27450

Yellow Brass Yes C27450 Profile
Suppliers of C27450

C27451

Yellow Brass (Yellow Brass) Yes C27451 Profile
Suppliers of C27451

C27460

Yes C27460 Profile
Suppliers of C27460

C28000 *

Muntz Metal, 60% Yes C28000 Profile
Suppliers of C28000

C37000

Free-Cutting Muntz Metal Yes C37000 Profile
Suppliers of C37000

C37100

Yes C37100 Profile
Suppliers of C37100

C38500

Architectural Bronze Yes C38500 Profile
Suppliers of C38500

C46400

Naval Brass, Uninhibited Yes C46400 Profile
Suppliers of C46400

C46500

Naval Brass, Arsenical Yes C46500 Profile
Suppliers of C46500

C46600

Tin Brass No C46600 Profile
Suppliers of C46600

C46700

Tin Brass No C46700 Profile
Suppliers of C46700

C46750

Yes C46750 Profile
Suppliers of C46750

C49300 *

Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile
Suppliers of C49300

C49355 *

Copper Zinc Bismuth Alloy Yes C49355 Profile
Suppliers of C49355

C49360 *

Tin-Eco(bismuth) Yes C49360 Profile
Suppliers of C49360

C62400 *

Aluminum Bronze,11% Yes C62400 Profile
Suppliers of C62400

C65100 *

Low-Silicon Bronze B Yes C65100 Profile
Suppliers of C65100

C65500 *

High-Silicon Bronze A Yes C65500 Profile
Suppliers of C65500