49 Alloys Found

Alloy UNS#DesignationActiveView

C15500 *

Yes C15500 Profile
Suppliers of C15500

C17200 *

Beryllium Copper Yes C17200 Profile
Suppliers of C17200

C17400 *

Beryllium Copper No C17400 Profile
Suppliers of C17400

C17410 *

Beryllium Copper Yes C17410 Profile
Suppliers of C17410

C17450 *

Beryllium Copper Yes C17450 Profile
Suppliers of C17450

C17455

Beryllium Copper Yes C17455 Profile
Suppliers of C17455

C17460 *

Beryllium Copper Yes C17460 Profile
Suppliers of C17460

C17465

Beryllium Copper Yes C17465 Profile
Suppliers of C17465

C18145

Yes C18145 Profile
Suppliers of C18145

C19002 *

Yes C19002 Profile
Suppliers of C19002

C19010 *

Yes C19010 Profile
Suppliers of C19010

C27450

Yellow Brass Yes C27450 Profile
Suppliers of C27450

C27451

Yellow Brass (Yellow Brass) Yes C27451 Profile
Suppliers of C27451

C27460

Yes C27460 Profile
Suppliers of C27460

C28000 *

Muntz Metal, 60% Yes C28000 Profile
Suppliers of C28000

C28340

Yes C28340 Profile
Suppliers of C28340

C28500

Copper-Zinc- Alloy (Brass) Yes C28500 Profile
Suppliers of C28500

C46400

Naval Brass, Uninhibited Yes C46400 Profile
Suppliers of C46400

C46500

Naval Brass, Arsenical Yes C46500 Profile
Suppliers of C46500

C46600

Tin Brass No C46600 Profile
Suppliers of C46600

C46700

Tin Brass No C46700 Profile
Suppliers of C46700

C49355 *

Copper Zinc Bismuth Alloy Yes C49355 Profile
Suppliers of C49355

C50590 *

Yes C50590 Profile
Suppliers of C50590

C50705 *

Yes C50705 Profile
Suppliers of C50705

C61900 *

Yes C61900 Profile
Suppliers of C61900

C62400 *

Aluminum Bronze,11% Yes C62400 Profile
Suppliers of C62400

C64760 *

Yes C64760 Profile
Suppliers of C64760

C67400

Yes C67400 Profile
Suppliers of C67400

C67420

Yes C67420 Profile
Suppliers of C67420

C67500

Manganese Bronze A Yes C67500 Profile
Suppliers of C67500

C67600

Yes C67600 Profile
Suppliers of C67600

C68800 *

Yes C68800 Profile
Suppliers of C68800

C69000 *

Copper Zinc No C69000 Profile
Suppliers of C69000

C69230 *

Yes C69230 Profile
Suppliers of C69230

C69240

Yes C69240 Profile
Suppliers of C69240

C69300 *

ECO Brass Yes C69300 Profile
Suppliers of C69300

C69310 *

SnEco Yes C69310 Profile
Suppliers of C69310

C69350

Yes C69350 Profile
Suppliers of C69350

C69400

Silicon Red Brass Yes C69400 Profile
Suppliers of C69400

C69410

Yes C69410 Profile
Suppliers of C69410

C69430

Yes C69430 Profile
Suppliers of C69430

C69750

Yes C69750 Profile
Suppliers of C69750

C69850

Yes C69850 Profile
Suppliers of C69850

C70260 *

Yes C70260 Profile
Suppliers of C70260

C70310 *

Yes C70310 Profile
Suppliers of C70310

C87850 *

Copper Silicon Alloy Yes C87850 Profile
Suppliers of C87850

C87860 *

Yes C87860 Profile
Suppliers of C87860

C87870 *

Yes C87870 Profile
Suppliers of C87870

C89841

Copper-Bismuth Alloy Yes C89841 Profile
Suppliers of C89841
* signifies an alloy registered with the U.S. EPA as Antimicrobial.