Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (32) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (31) You Searched For: capacity-for-being-cold-worked:"Excellent" elongation:[48 TO 51] elongation:[24 TO 27] CLEAR this search X SAVE this search << Page 1 >> 34 Alloys Found Alloy UNS#DesignationActiveView C10100 * Oxygen-Free-Electronic (OFE) Yes C10100 Profile Suppliers of C10100 C10200 * Oxygen-Free (OF) Yes C10200 Profile Suppliers of C10200 C10300 * Oxygen-Free Copper (OFXLP) Yes C10300 Profile Suppliers of C10300 C10400 * Oxygen-Free with Ag (OFS) Yes C10400 Profile Suppliers of C10400 C10500 * Oxygen-Free with Ag (OFS) Yes C10500 Profile Suppliers of C10500 C10700 * Oxygen-Free with Ag (OFS) Yes C10700 Profile Suppliers of C10700 C10800 * Yes C10800 Profile Suppliers of C10800 C10910 * Yes C10910 Profile Suppliers of C10910 C11000 * Electrolytic Tough Pitch (ETP) Yes C11000 Profile Suppliers of C11000 C11300 * Tough Pitch with Ag (STP) Yes C11300 Profile Suppliers of C11300 C11400 * Tough Pitch with Ag (STP) Yes C11400 Profile Suppliers of C11400 C11500 * Tough Pitch with Ag (STP) Yes C11500 Profile Suppliers of C11500 C11600 * Tough Pitch with Ag (STP) Yes C11600 Profile Suppliers of C11600 C12000 * Phosphorus-Deoxidized, Low Residual P (DLP) Yes C12000 Profile Suppliers of C12000 C12100 * Phosphorus-Deoxidized, Low Residual P (DLPS) Yes C12100 Profile Suppliers of C12100 C12200 * Phosphorus-Deoxidized, High Residual P (DHP) Yes C12200 Profile Suppliers of C12200 C12210 * Yes C12210 Profile Suppliers of C12210 C15000 * Zirconium Copper Yes C15000 Profile Suppliers of C15000 C18200 Chromium Copper Yes C18200 Profile Suppliers of C18200 C18400 Chromium Copper Yes C18400 Profile Suppliers of C18400 C18500 High Copper No C18500 Profile Suppliers of C18500 C19000 * Yes C19000 Profile Suppliers of C19000 C22000 * Commercial Bronze, 90% Yes C22000 Profile Suppliers of C22000 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C50580 * Yes C50580 Profile Suppliers of C50580 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51100 * Yes C51100 Profile Suppliers of C51100 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>