Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (41) Inactive Alloys (3) U.S. EPA Registered Antimicrobial (24) You Searched For: elongation:[18 TO 21] rockwell-b-scale:[70 TO 80] tensile-strength:[* TO 50] CLEAR this search X SAVE this search << Page 1 >> 44 Alloys Found Alloy UNS#DesignationActiveView C15000 * Zirconium Copper Yes C15000 Profile Suppliers of C15000 C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C17510 * Copper Beryllium Yes C17510 Profile Suppliers of C17510 C18200 Chromium Copper Yes C18200 Profile Suppliers of C18200 C18400 Chromium Copper Yes C18400 Profile Suppliers of C18400 C18500 High Copper No C18500 Profile Suppliers of C18500 C18625 * HRSC Yes C18625 Profile Suppliers of C18625 C19200 * Yes C19200 Profile Suppliers of C19200 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C33500 Low-Leaded Brass Yes C33500 Profile Suppliers of C33500 C34000 Medium Leaded Brass, 64-1/2% Yes C34000 Profile Suppliers of C34000 C34200 High Leaded Brass, 64-1/2% Yes C34200 Profile Suppliers of C34200 C34500 Yes C34500 Profile Suppliers of C34500 C35000 Medium Leaded Brass, 62% Yes C35000 Profile Suppliers of C35000 C35300 High Leaded Brass, 62% Yes C35300 Profile Suppliers of C35300 C35330 DZR Brass Yes C35330 Profile Suppliers of C35330 C35600 Extra High Leaded Brass Yes C35600 Profile Suppliers of C35600 C36000 Free-Cutting Brass Yes C36000 Profile Suppliers of C36000 C36010 Leaded Brass (Free-Cutting Brass) Yes C36010 Profile Suppliers of C36010 C36200 Leaded Brass No C36200 Profile Suppliers of C36200 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C42500 * Yes C42500 Profile Suppliers of C42500 C43400 * Yes C43400 Profile Suppliers of C43400 C46400 Naval Brass, Uninhibited Yes C46400 Profile Suppliers of C46400 C48200 Naval Brass, Medium Leaded Yes C48200 Profile Suppliers of C48200 C48500 Naval Brass, High Leaded Yes C48500 Profile Suppliers of C48500 C48600 DZR Brass Yes C48600 Profile Suppliers of C48600 C48645 Yes C48645 Profile Suppliers of C48645 C54400 Phosphor Bronze B-2 Yes C54400 Profile Suppliers of C54400 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 C65500 * High-Silicon Bronze A Yes C65500 Profile Suppliers of C65500 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 C70400 * Copper-Nickel, 5% Yes C70400 Profile Suppliers of C70400 C71000 * Copper-Nickel, 20% Yes C71000 Profile Suppliers of C71000 C82000 * Copper Beryllium 10C Yes C82000 Profile Suppliers of C82000 C82200 * Copper Beryllium 3C Yes C82200 Profile Suppliers of C82200 C87610 * Cast Copper-Silicon Yes C87610 Profile Suppliers of C87610 C89720 * Copper-Bismuth Alloy (TECO) Yes C89720 Profile Suppliers of C89720 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>