Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (60) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (61) You Searched For: coated-metal-arc-welding:"Not Recommended" element_names:"Zinc" antimicrobial:"true" CLEAR this search X SAVE this search << Page 1 2 >> 61 Alloys Found Alloy UNS#DesignationActiveView C10100 * Oxygen-Free-Electronic (OFE) Yes C10100 Profile Suppliers of C10100 C12510 * Yes C12510 Profile Suppliers of C12510 C19000 * Yes C19000 Profile Suppliers of C19000 C19040 * CAC5 (High Copper) Yes C19040 Profile Suppliers of C19040 C19050 * SPKFC-5E (High Copper) Yes C19050 Profile Suppliers of C19050 C19170 * KLF170 (High Copper) Yes C19170 Profile Suppliers of C19170 C19200 * Yes C19200 Profile Suppliers of C19200 C19215 * Yes C19215 Profile Suppliers of C19215 C19240 * Super KFC Yes C19240 Profile Suppliers of C19240 C19250 * SPKFC-5W (High Copper) Yes C19250 Profile Suppliers of C19250 C19280 * Yes C19280 Profile Suppliers of C19280 C19400 * Yes C19400 Profile Suppliers of C19400 C19419 * CAC19 (High Copper) Yes C19419 Profile Suppliers of C19419 C21000 * Gilding, 95% Yes C21000 Profile Suppliers of C21000 C22000 * Commercial Bronze, 90% Yes C22000 Profile Suppliers of C22000 C22600 * Jewelry Bronze, 87-1/2% Yes C22600 Profile Suppliers of C22600 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C23400 * Yes C23400 Profile Suppliers of C23400 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C27400 * Yellow Brass, 63% Yes C27400 Profile Suppliers of C27400 C28000 * Muntz Metal, 60% Yes C28000 Profile Suppliers of C28000 C40500 * Penny Bronze Yes C40500 Profile Suppliers of C40500 C41100 * Tin Brass Yes C41100 Profile Suppliers of C41100 C41120 * Yes C41120 Profile Suppliers of C41120 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C41500 * Tin Brass Yes C41500 Profile Suppliers of C41500 C42500 * Yes C42500 Profile Suppliers of C42500 C42520 * Yes C42520 Profile Suppliers of C42520 C42600 * Yes C42600 Profile Suppliers of C42600 C43000 * Tin Brass Yes C43000 Profile Suppliers of C43000 C43500 * Tin Brass Yes C43500 Profile Suppliers of C43500 C44300 * Admiralty, Arsenical Yes C44300 Profile Suppliers of C44300 C44400 * Admiralty, Antimonial Yes C44400 Profile Suppliers of C44400 C44500 * Admiralty, Phosphorized Yes C44500 Profile Suppliers of C44500 C64740 * Yes C64740 Profile Suppliers of C64740 C64770 * Yes C64770 Profile Suppliers of C64770 C66420 * Yes C66420 Profile Suppliers of C66420 C66430 * Yes C66430 Profile Suppliers of C66430 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 C68300 * Copper-Znc Alloy (Silicon Modified Brass) Yes C68300 Profile Suppliers of C68300 C68700 * Aluminum Brass, Arsenical Yes C68700 Profile Suppliers of C68700 C69100 * Yes C69100 Profile Suppliers of C69100 C70240 * Yes C70240 Profile Suppliers of C70240 C73500 * Nickel Silver Yes C73500 Profile Suppliers of C73500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 2 >>