Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (51) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (39) You Searched For: density:[0.31 TO 0.32] capacity-for-being-cold-worked:"Excellent" element_names:"Tin" CLEAR this search X SAVE this search << Page 1 2 >> 52 Alloys Found Alloy UNS#DesignationActiveView C17460 * Copper Beryllium Yes C17460 Profile Suppliers of C17460 C17465 Copper Beryllium Yes C17465 Profile Suppliers of C17465 C18090 Yes C18090 Profile Suppliers of C18090 C18625 * HRSC Yes C18625 Profile Suppliers of C18625 C19720 * Yes C19720 Profile Suppliers of C19720 C27453 Copper Zinc Alloy Yes C27453 Profile Suppliers of C27453 C27460 Yes C27460 Profile Suppliers of C27460 C28340 Yes C28340 Profile Suppliers of C28340 C40500 * Penny Bronze Yes C40500 Profile Suppliers of C40500 C40800 * Silicon Brass No C40800 Profile Suppliers of C40800 C40810 * Yes C40810 Profile Suppliers of C40810 C40850 * Yes C40850 Profile Suppliers of C40850 C40860 * Yes C40860 Profile Suppliers of C40860 C40950 * Yes C40950 Profile Suppliers of C40950 C41100 * Tin Brass Yes C41100 Profile Suppliers of C41100 C41120 * Yes C41120 Profile Suppliers of C41120 C41125 * Yes C41125 Profile Suppliers of C41125 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C41500 * Tin Brass Yes C41500 Profile Suppliers of C41500 C42200 * Yes C42200 Profile Suppliers of C42200 C42210 * Tin Brass Yes C42210 Profile Suppliers of C42210 C42220 * Yes C42220 Profile Suppliers of C42220 C42230 Yes C42230 Profile Suppliers of C42230 C42500 * Yes C42500 Profile Suppliers of C42500 C42520 * Yes C42520 Profile Suppliers of C42520 C42600 * Yes C42600 Profile Suppliers of C42600 C43000 * Tin Brass Yes C43000 Profile Suppliers of C43000 C43400 * Yes C43400 Profile Suppliers of C43400 C43500 * Tin Brass Yes C43500 Profile Suppliers of C43500 C49100 Yes C49100 Profile Suppliers of C49100 C50780 * Yes C50780 Profile Suppliers of C50780 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51080 * Yes C51080 Profile Suppliers of C51080 C51100 * Yes C51100 Profile Suppliers of C51100 C51180 * Yes C51180 Profile Suppliers of C51180 C51900 * Yes C51900 Profile Suppliers of C51900 C51980 * Yes C51980 Profile Suppliers of C51980 C64740 * Yes C64740 Profile Suppliers of C64740 C64751 Yes C64751 Profile Suppliers of C64751 C64752 Yes C64752 Profile Suppliers of C64752 C64810 NKC4820 Yes C64810 Profile Suppliers of C64810 C66200 * Yes C66200 Profile Suppliers of C66200 C66430 * Yes C66430 Profile Suppliers of C66430 C69150 * Copper Zinc Alloy (Copper Zinc Alloy) Yes C69150 Profile Suppliers of C69150 C69750 Yes C69750 Profile Suppliers of C69750 C70255 Yes C70255 Profile Suppliers of C70255 C70265 * Yes C70265 Profile Suppliers of C70265 C70290 * Yes C70290 Profile Suppliers of C70290 C70310 * Yes C70310 Profile Suppliers of C70310 C72660 * Yes C72660 Profile Suppliers of C72660 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 2 >>