36 Alloys Found

Alloy UNS#DesignationActiveView

C24000 *

Low Brass, 80% Yes C24000 Profile
Suppliers of C24000

C26000 *

Cartridge Brass, 70% Yes C26000 Profile
Suppliers of C26000

C26100 *

Brass No C26100 Profile
Suppliers of C26100

C26130 *

Yes C26130 Profile
Suppliers of C26130

C26200 *

Yes C26200 Profile
Suppliers of C26200

C26800 *

Yellow Brass, 66% Yes C26800 Profile
Suppliers of C26800

C27000 *

Yellow Brass, 65% Yes C27000 Profile
Suppliers of C27000

C27400 *

Yellow Brass, 63% Yes C27400 Profile
Suppliers of C27400

C27450

Yellow Brass Yes C27450 Profile
Suppliers of C27450

C27451

Yellow Brass (Yellow Brass) Yes C27451 Profile
Suppliers of C27451

C27453

Copper Zinc Alloy Yes C27453 Profile
Suppliers of C27453

C27460

Yes C27460 Profile
Suppliers of C27460

C33000

Low Leaded Brass (Tube) Yes C33000 Profile
Suppliers of C33000

C33100

Leaded Brass No C33100 Profile
Suppliers of C33100

C33200

High Leaded Brass (Tube) Yes C33200 Profile
Suppliers of C33200

C41300 *

Tin Brass Yes C41300 Profile
Suppliers of C41300

C42520 *

Yes C42520 Profile
Suppliers of C42520

C43500 *

Tin Brass Yes C43500 Profile
Suppliers of C43500

C44300 *

Admiralty, Arsenical Yes C44300 Profile
Suppliers of C44300

C44400 *

Admiralty, Antimonial Yes C44400 Profile
Suppliers of C44400

C44500 *

Admiralty, Phosphorized Yes C44500 Profile
Suppliers of C44500

C51000 *

Phosphor Bronze, 5% A Yes C51000 Profile
Suppliers of C51000

C51080 *

Yes C51080 Profile
Suppliers of C51080

C51100 *

Yes C51100 Profile
Suppliers of C51100

C51180 *

Yes C51180 Profile
Suppliers of C51180

C51900 *

Yes C51900 Profile
Suppliers of C51900

C51980 *

Yes C51980 Profile
Suppliers of C51980

C63600

Yes C63600 Profile
Suppliers of C63600

C65500 *

High-Silicon Bronze A Yes C65500 Profile
Suppliers of C65500

C66430 *

Yes C66430 Profile
Suppliers of C66430

C66700 *

Manganese Brass Yes C66700 Profile
Suppliers of C66700

C68350 *

Low Silicon Brass Yes C68350 Profile
Suppliers of C68350

C68700 *

Aluminum Brass, Arsenical Yes C68700 Profile
Suppliers of C68700

C69750

Yes C69750 Profile
Suppliers of C69750

C72600 *

Copper Nickel No C72600 Profile
Suppliers of C72600

C74400 *

Nickel Silver Yes C74400 Profile
Suppliers of C74400
* signifies an alloy registered with the U.S. EPA as Antimicrobial.