899 Alloys Found

Alloy UNS#DesignationActiveView

C87520

Copper Silicon No C87520 Profile
Suppliers of C87520

C87530

Copper Silicon No C87530 Profile
Suppliers of C87530

C87600 *

Copper Silcon Alloy Yes C87600 Profile
Suppliers of C87600

C87610 *

Cast Copper-Silicon Yes C87610 Profile
Suppliers of C87610

C87700 *

Silicon Bronze (Silicon Bronze) Yes C87700 Profile
Suppliers of C87700

C87710 *

Silicon Bronze (Silicon Bronze) Yes C87710 Profile
Suppliers of C87710

C87800 *

Cast Silicon Bronze Yes C87800 Profile
Suppliers of C87800

C87845 *

Copper-Silicon-Brass Yes C87845 Profile
Suppliers of C87845

C87850 *

Copper Silicon Alloy Yes C87850 Profile
Suppliers of C87850

C87860 *

Yes C87860 Profile
Suppliers of C87860

C87870 *

Yes C87870 Profile
Suppliers of C87870

C87900

Copper Silicon Yes C87900 Profile
Suppliers of C87900

C89320 *

Yes C89320 Profile
Suppliers of C89320

C89325

Yes C89325 Profile
Suppliers of C89325

C89510 *

SeBiLOY I (EnviroBrass I) Yes C89510 Profile
Suppliers of C89510

C89520 *

SeBiLOY II (EnviroBrass II) Yes C89520 Profile
Suppliers of C89520

C89530

Copper-Bismuth-Selenium Alloy (Brasses) Yes C89530 Profile
Suppliers of C89530

C89535

Copper-Bismuth Alloy Yes C89535 Profile
Suppliers of C89535

C89537 *

Yes C89537 Profile
Suppliers of C89537

C89540

Yes C89540 Profile
Suppliers of C89540

C89545

Yes C89545 Profile
Suppliers of C89545

C89550 *

SeBiLOY III (EnviroBrass III) Yes C89550 Profile
Suppliers of C89550

C89560 *

Copper-Zinc-Bismuth Yes C89560 Profile
Suppliers of C89560

C89570 *

Yes C89570 Profile
Suppliers of C89570

C89580 *

Yes C89580 Profile
Suppliers of C89580

C89710

Green Brass Yes C89710 Profile
Suppliers of C89710

C89720 *

Copper-Bismuth Alloy (TECO) Yes C89720 Profile
Suppliers of C89720

C89831

Yes C89831 Profile
Suppliers of C89831

C89833 *

Copper Bismuth Alloy Yes C89833 Profile
Suppliers of C89833

C89835 *

Federalloy III-932 Yes C89835 Profile
Suppliers of C89835

C89836

Copper Bismuth Alloy Yes C89836 Profile
Suppliers of C89836

C89837

Yes C89837 Profile
Suppliers of C89837

C89838

Yes C89838 Profile
Suppliers of C89838

C89839

Yes C89839 Profile
Suppliers of C89839

C89841

Copper-Bismuth Alloy Yes C89841 Profile
Suppliers of C89841

C89842 *

Copper-Zinc-Tin-Bismuth Yes C89842 Profile
Suppliers of C89842

C89844

Yes C89844 Profile
Suppliers of C89844

C89845 *

Copper-Bismuth-Alloy Yes C89845 Profile
Suppliers of C89845

C89940 *

Yes C89940 Profile
Suppliers of C89940

C90200

Yes C90200 Profile
Suppliers of C90200

C90250

Tin Bronze No C90250 Profile
Suppliers of C90250

C90280 *

Yes C90280 Profile
Suppliers of C90280

C90300

Tin Bronze Yes C90300 Profile
Suppliers of C90300

C90400 *

Tin Bronze Yes C90400 Profile
Suppliers of C90400

C90410 *

Tin Bronze Yes C90410 Profile
Suppliers of C90410

C90420 *

Tin Bronze Yes C90420 Profile
Suppliers of C90420

C90430 *

Low-Lead Tin Bronze Yes C90430 Profile
Suppliers of C90430

C90500

Gun Metal Yes C90500 Profile
Suppliers of C90500

C90700

Tin Bronze, 65 Yes C90700 Profile
Suppliers of C90700

C90710

Yes C90710 Profile
Suppliers of C90710
* signifies an alloy registered with the U.S. EPA as Antimicrobial.