Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (38) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (33) You Searched For: yield-strength:[50 TO 70] melting-point-solidus:[1900 TO 1950] CLEAR this search X SAVE this search << Page 1 >> 40 Alloys Found Alloy UNS#DesignationActiveView C12500 * Fire-Refined Tough Pitch (FRTP) Yes C12500 Profile Suppliers of C12500 C12510 * Yes C12510 Profile Suppliers of C12510 C14300 * Cadmium Copper, Deoxidized Yes C14300 Profile Suppliers of C14300 C14310 * Cadmium Copper No C14310 Profile Suppliers of C14310 C14500 * Tellurium-Bearing (PTE) Yes C14500 Profile Suppliers of C14500 C14510 * Tellurium-Bearing Yes C14510 Profile Suppliers of C14510 C14520 * Phosphorus-Deoxidized,Tellurium-Bearing (DPTE) Yes C14520 Profile Suppliers of C14520 C14530 * Yes C14530 Profile Suppliers of C14530 C19000 * Yes C19000 Profile Suppliers of C19000 C19005 Yes C19005 Profile Suppliers of C19005 C19100 Yes C19100 Profile Suppliers of C19100 C19140 Yes C19140 Profile Suppliers of C19140 C19160 Yes C19160 Profile Suppliers of C19160 C19215 * Yes C19215 Profile Suppliers of C19215 C19217 Yes C19217 Profile Suppliers of C19217 C19419 * CAC19 (High Copper) Yes C19419 Profile Suppliers of C19419 C19800 * Yes C19800 Profile Suppliers of C19800 C19810 * Hig Copper Alloy Yes C19810 Profile Suppliers of C19810 C21000 * Gilding, 95% Yes C21000 Profile Suppliers of C21000 C40800 * Silicon Brass No C40800 Profile Suppliers of C40800 C40820 * Yes C40820 Profile Suppliers of C40820 C40950 * Yes C40950 Profile Suppliers of C40950 C50500 * Phosphor Bronze, 1.25% E Yes C50500 Profile Suppliers of C50500 C50580 * Yes C50580 Profile Suppliers of C50580 C50590 * Yes C50590 Profile Suppliers of C50590 C61300 * Yes C61300 Profile Suppliers of C61300 C61400 * Yes C61400 Profile Suppliers of C61400 C61900 * Yes C61900 Profile Suppliers of C61900 C62300 * Aluminum Bronze, 9% Yes C62300 Profile Suppliers of C62300 C62500 * Yes C62500 Profile Suppliers of C62500 C63200 * Aluminum Bronze Yes C63200 Profile Suppliers of C63200 C64725 * Copper Silicon Alloy Yes C64725 Profile Suppliers of C64725 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 C70260 * Yes C70260 Profile Suppliers of C70260 C70275 * Copper Nickel Alloy (MAX126) Yes C70275 Profile Suppliers of C70275 C70315 STOL 94 Yes C70315 Profile Suppliers of C70315 C72500 * Yes C72500 Profile Suppliers of C72500 C75400 Nickel Silver, 65-15 Yes C75400 Profile Suppliers of C75400 C95500 * Yes C95500 Profile Suppliers of C95500 C95800 * Yes C95800 Profile Suppliers of C95800 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>