53 Alloys Found

Alloy UNS#DesignationActiveView

C10300 *

Oxygen-Free Copper (OFXLP) Yes C10300 Profile
Suppliers of C10300

C10800 *

Yes C10800 Profile
Suppliers of C10800

C12000 *

Phosphorus-Deoxidized, Low Residual P (DLP) Yes C12000 Profile
Suppliers of C12000

C12100 *

Phosphorus-Deoxidized, Low Residual P (DLPS) Yes C12100 Profile
Suppliers of C12100

C12200 *

Phosphorus-Deoxidized, High Residual P (DHP) Yes C12200 Profile
Suppliers of C12200

C12210 *

Yes C12210 Profile
Suppliers of C12210

C14300 *

Cadmium Copper, Deoxidized Yes C14300 Profile
Suppliers of C14300

C14310 *

Cadmium Copper No C14310 Profile
Suppliers of C14310

C14425

Copper (Copper) Yes C14425 Profile
Suppliers of C14425

C14530 *

Yes C14530 Profile
Suppliers of C14530

C18090

Yes C18090 Profile
Suppliers of C18090

C18900 *

Yes C18900 Profile
Suppliers of C18900

C19022 *

High Copper Alloy Yes C19022 Profile
Suppliers of C19022

C19200 *

Yes C19200 Profile
Suppliers of C19200

C19215 *

Yes C19215 Profile
Suppliers of C19215

C19220 *

Yes C19220 Profile
Suppliers of C19220

C19280 *

Yes C19280 Profile
Suppliers of C19280

C19400 *

Yes C19400 Profile
Suppliers of C19400

C40810 *

Yes C40810 Profile
Suppliers of C40810

C42200 *

Yes C42200 Profile
Suppliers of C42200

C42210 *

Tin Brass Yes C42210 Profile
Suppliers of C42210

C42220 *

Yes C42220 Profile
Suppliers of C42220

C61300 *

Yes C61300 Profile
Suppliers of C61300

C61500 *

Yes C61500 Profile
Suppliers of C61500

C61900 *

Yes C61900 Profile
Suppliers of C61900

C63200 *

Aluminum Bronze Yes C63200 Profile
Suppliers of C63200

C63800 *

Yes C63800 Profile
Suppliers of C63800

C64740 *

Yes C64740 Profile
Suppliers of C64740

C65100 *

Low-Silicon Bronze B Yes C65100 Profile
Suppliers of C65100

C65400

Yes C65400 Profile
Suppliers of C65400

C65500 *

High-Silicon Bronze A Yes C65500 Profile
Suppliers of C65500

C66908 *

Copper-Zinc-Manganese Yes C66908 Profile
Suppliers of C66908

C66910 *

Copper-Zinc-Manganese Yes C66910 Profile
Suppliers of C66910

C66913 *

Copper-Zinc-Manganese Yes C66913 Profile
Suppliers of C66913

C66915 *

Copper-Zinc-Manganese Yes C66915 Profile
Suppliers of C66915

C70400 *

Copper-Nickel, 5% Yes C70400 Profile
Suppliers of C70400

C70600 *

Copper-Nickel, 10% Yes C70600 Profile
Suppliers of C70600

C71000 *

Copper-Nickel, 20% Yes C71000 Profile
Suppliers of C71000

C71500 *

Copper-Nickel, 30% Yes C71500 Profile
Suppliers of C71500

C72200

Yes C72200 Profile
Suppliers of C72200

C72600 *

Copper Nickel No C72600 Profile
Suppliers of C72600

C72700 *

Yes C72700 Profile
Suppliers of C72700

C72800 *

Yes C72800 Profile
Suppliers of C72800

C72900 *

Yes C72900 Profile
Suppliers of C72900

C87300 *

Silicon Bronze Yes C87300 Profile
Suppliers of C87300

C87500 *

Coppe Silicon Alloy Yes C87500 Profile
Suppliers of C87500

C87600 *

Copper Silcon Alloy Yes C87600 Profile
Suppliers of C87600

C87610 *

Cast Copper-Silicon Yes C87610 Profile
Suppliers of C87610

C87800 *

Cast Silicon Bronze Yes C87800 Profile
Suppliers of C87800

C95200 *

Yes C95200 Profile
Suppliers of C95200
* signifies an alloy registered with the U.S. EPA as Antimicrobial.